Standards |
Grade |
Size
|
Process |
Surface condition |
Heat treatment |
Mechanical property |
HB |
Remarks |
LF |
VD |
ESR |
SB |
SG |
RT |
TN |
TA |
SC |
σb
Mpa |
σs
Mpa |
δ5
% |
ψ
% |
Akv
J |
max |
min |
GB/T3203-1982 |
G20CrNiMo |
80-460 |
√ |
√ |
- |
× |
√ |
- |
- |
√ |
× |
120 |
|
9 |
45 |
8 |
|
|
Size of sample:15,M is after TQT |
GB/T3203-1982 |
G20CrNi2Mo |
80-460 |
√ |
√ |
- |
× |
√ |
- |
- |
√ |
× |
100 |
|
13 |
45 |
8 |
|
|
Size of sample:25,M is after TQT |
GB/T3203-1982 |
G20Cr2Ni4 |
80-460 |
√ |
√ |
- |
× |
√ |
- |
- |
√ |
× |
120 |
|
10 |
45 |
8 |
|
|
Size of sample:15,M is after TQT |
GB/T3077-1999 |
20CrMnTi |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
1080 |
850 |
10 |
45 |
55 |
217 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
30CrMnTi |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
1470 |
|
9 |
40 |
47 |
229 |
|
Sampling,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20CrNiMo |
80-520 |
√ |
√ |
- |
- |
√ |
- |
- |
√ |
- |
980 |
785 |
9 |
40 |
47 |
197 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20CrMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
885 |
685 |
12 |
50 |
78 |
197 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
42CrMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
1080 |
930 |
12 |
45 |
63 |
217 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20Cr |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
835 |
540 |
10 |
40 |
47 |
179 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
40Cr |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
980 |
785 |
9 |
45 |
47 |
207 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
35CrMoV |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
1080 |
930 |
10 |
50 |
71 |
241 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
12CrMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
410 |
265 |
24 |
60 |
110 |
179 |
|
Size of sample:30mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
15CrMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
√ |
440 |
295 |
22 |
60 |
94 |
179 |
|
Size of sample:30mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB1591-88 |
20CrV |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
835 |
590 |
12 |
45 |
55 |
197 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
40CrV |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
885 |
735 |
10 |
50 |
71 |
241 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20MnV |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
785 |
590 |
10 |
40 |
55 |
187 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20CrMnMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
- |
1180 |
885 |
10 |
45 |
55 |
217 |
|
Size of sample:15mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
40CrMnMo |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
- |
- |
980 |
785 |
10 |
45 |
63 |
217 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
20CrMnSi |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
785 |
635 |
12 |
45 |
55 |
207 |
|
Size of sample:25mm,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
GB/T3077-1999 |
35CrMnSiA |
80-520 |
√ |
- |
- |
√ |
- |
- |
- |
√ |
- |
1620 |
1280 |
9 |
40 |
31 |
229 |
|
Sampling,Mechanical property is after quenching and tempering,HB is after annealing/tempering |
|
|
Electroslag remelting-ESR,Black Condition-SB,Grindering-SG,Rough Turned-RT,Normalizing-TN,Annealing-TA,Soft Cooling-SC,
tensile strength-σb Mpa,yield strength-σsMpa,elongation percentage-δ5%,reduction of area-ψ%,Charpy Impact-AkvJ,Brinell hardness-HB |
|
|
|
|
Company Name: Wuhan Xingfangyuan Import and Export Co.,Ltdh
Address: A2903#,Building A, Sanyang Plaza,Sanyang Road, Jiang'an District,Wuhan,Hubei Province Postalcode: 430019
Tel: +86-18062029576 Skype: snowysky28
Email: lucy@qilut.com
Technology: jingluntech |
|
|
|